Fenómeno del problema
Delamination or poor interface appears in K-RESIN and PS blended products
Análisis de la causa
Limited compatibility between K-RESIN and PS, weak interfacial bonding Improper compounding temperature (deviating from 200-240°C) Improper K-RESIN/PS ratio Insufficient compounding time, uneven dispersion Shrinkage rate difference between the two materials causes interfacial stress
Solución
Optimize K-RESIN/PS ratio Strictly control compounding temperature according to the 200-240°C range Extend compounding time to ensure dispersion Add compatibilizer to improve the interface Consider shrinkage rate difference in design
Conclusión clave
K-RESIN/PS blending needs to optimize ratio and compatibility
K resinPS blendinginterfacecompatibility