Unstable transparency of K-RESIN injection products

Fenómeno del problema
Transparency of K-RESIN injection products is unstable, with obvious haze differences between batches
Análisis de la causa
Barrel temperature fluctuation causes K-RESIN microstructure changes Injection speed too fast produces orientation affecting transparency Poor mold venting, gas interferes with transparency High raw material moisture content Improper gate design produces turbulence
Solución
Stabilize barrel temperature within the 200-240°C range Appropriately reduce injection speed to reduce orientation Improve mold venting Fully dry raw material Optimize gate design, use fan gates
Conclusión clave
K-RESIN transparency needs stable temperature and venting
K resintransparencyinjection stability