Material Drying 7 visualizações

Unstable transparency of K-RESIN injection products

Fenómeno do problema
Transparency of K-RESIN injection products is unstable, with obvious haze differences between batches
Análise das causas
Barrel temperature fluctuation causes K-RESIN microstructure changes Injection speed too fast produces orientation affecting transparency Poor mold venting, gas interferes with transparency High raw material moisture content Improper gate design produces turbulence
Solução
Stabilize barrel temperature within the 200-240°C range Appropriately reduce injection speed to reduce orientation Improve mold venting Fully dry raw material Optimize gate design, use fan gates
Conclusão principal
K-RESIN transparency needs stable temperature and venting