Extrusion & Post
10 visualizaciones
PAN fiber fracture during drawing
Fenómeno del problema
Fibers break during steam drawing or hot drawing
Análisis de la causa
Drawing temperature too low, PAN molecular chain mobility insufficient; draw ratio too large exceeding the drawing limit
Solución
Appropriately increase the drawing temperature (steam 100-120°C or dry heat drawing); draw in multiple stages to gradually increase the draw ratio
Conclusión clave
PAN drawing is the key to improving carbon fiber orientation and strength