Molding Process
15 visualizaciones
Product surface yellowing
Fenómeno del problema
The product color obviously darkens after processing
Análisis de la causa
Processing temperature exceeding 370°C causes thermo-oxidation generating chromophores; material residence time too long accumulating thermal history
Solución
Reduce the melt temperature by 10-20°C to the safe window; reduce residence time; increase antioxidant dosage
Conclusión clave
The yellowing of PES is a direct manifestation of thermo-oxidation