Q
POE processing moisture causes silver streaks
A
Silver streaks are caused by moisture vaporization and stretching; drying and venting are the main countermeasures
Material Drying POE injectionsilver streakmoisture dryingventingback pressure
Q
POE '2079851475616104452 cold slug marks
A
Cold slug marks are caused by solidified residual material in the nozzle; raising nozzle temperature and cold slug well design are key
Injection Molding POE injectioncold slug marknozzle temperaturecold slug wellinjection pressure
Q
POE toughened PP low-temperature impact insufficient
A
Low-temperature toughening requires lower Tg and stronger interfacial adhesion
Molding Process POE low-temperature tougheningimpact strengthTgPOE-g-MAHEPDM
Q
POE extrusion film winding wrinkling
A
Film wrinkling is caused by tension fluctuation and uneven thickness; automatic tension control and uniformization are key
Extrusion & Post POE filmwinding wrinklingtension controlthickness uniformityguide roller parallelism
Q
POE '2079851475616104452 flow marks
A
Flow marks are caused by unstable injection front and rapid cooling; multi-stage injection and high mold temperature are key
Injection Molding POE injectionflow markinjection speedmold temperaturegate area
Q
POE '2079851475616104452 sink marks
A
Sink marks are caused by insufficient holding and wall thickness difference; high-pressure holding and multiple gates are core countermeasures
Injection Molding POE injectionsink markholding pressurewall thickness differencegate design
Q
POE repeated processing performance decay
A
Performance decay from multiple processing is caused by thermo-mechanical degradation; limiting regrind and supplementing antioxidant are key
Production & Quality POE recyclingperformance decayantioxidant supplementthermal degradationshear degradation
Q
POE toughened PP impact strength not up to standard
A
The key to POE toughened PP is dispersed phase 0.2-0.5μm and interfacial adhesion
Molding Process POE toughened PPimpact strengthdispersed phase particle sizePOE-g-MAHsilver streak shear band
Q
POE '2079851475616104452 multi-cavity filling imbalance
A
Multi-cavity filling imbalance is caused by runner design; balanced runners and mold flow analysis are key
Injection Molding POE injectionmulti-cavity balancerunner designgate sizemold flow analysis
Q
POE injection molded product ejector pin whitening