Material Drying
3 조회수
PLA Deep Dehumidification 85℃
문제 현상
After ordinary drying, PLA extrusion still has filament breakage and bubbles, and the moisture content test still exceeds the standard
원인 분석
Deep moisture in PLA requires low dew point and long dehumidification: fine-denier fiber standards require 85±0.5℃, dew point ≤-55℃, and 4 hours of residence, only then can the moisture content be pressed below 30ppm
해결 방법
①For high-requirement processes use 85℃×4h, dew point ≤-55℃ deep dehumidification; ②Dual molecular sieve rotor redundant configuration; ③Microwave moisture meter real-time feedback; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
Drying for high-requirement PLA processing is system engineering; dew point -55℃ plus 4 hours of residence is the equipment guarantee for ppm-level moisture; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!