문제 현상
PSU metal insert products show poor interfacial bonding and stress cracking; failure after thermal cycling.
원인 분석
Thermal expansion difference between PSU and metal; insufficient insert preheating; molding stress concentrates at the interface; thermal cycling stress accumulates.; During on-site troubleshooting, verify item by item according to this mechanism, avoiding blindly adjusting the machine based solely on experience
해결 방법
①Fully preheat inserts; ②Mechanical interlock design at the interface; ③Low-stress molding; ④Thermal cycling verification.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
PSU insert parts require management of thermal expansion mismatch; preheating and interlocking are standard means; cyclic verification exposes long-term risks.; After confirming effectiveness, solidify the parameters and practices into the work instructions to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!