Thin flash appears at the parting line or moving parts of the product

문제 현상
Thin flash appears at the parting line or moving parts of the product, affecting appearance and dimensional accuracy, mold mating marks visible at the flash
원인 분석
Injection pressure too high, exceeding the mold clamping force Mold mating surfaces worn or machining accuracy insufficient Barrel temperature too high (170-230°C on the high side), low melt viscosity, excessively strong flowability Holding pressure too high, time too long Clamping force insufficient
해결 방법
Reduce injection pressure to a reasonable range Repair mold mating surfaces to ensure accuracy Appropriately lower barrel temperature to the low side of 170-230°C Reduce holding pressure and time Increase clamping force or change to a larger machine
핵심 요약
Flash requires controlling injection pressure, temperature and clamping force