Material Drying
4 조회수
The low peel strength problem of PBAK acrylate type in drying
문제 현상
Polybutyl acrylate-type PBAK exhibited low peel strength during drying processing at 80-150°C.
원인 분석
Improper crosslinking degree of PBAK caused the problem.
해결 방법
Improve the drying method.
핵심 요약
PBAK for coating and adhesive applications requires fine formulation design.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다