Material Drying 3 Aufrufe

The low peel strength problem of PBAK acrylate type in drying

Problembeschreibung
Polybutyl acrylate-type PBAK exhibited low peel strength during drying processing at 80-150°C.
Ursachenanalyse
Improper crosslinking degree of PBAK caused the problem.
Lösung
Improve the drying method.
Wichtigste Erkenntnis
PBAK for coating and adhesive applications requires fine formulation design.