Material Drying
2 views
The low peel strength problem of PBAK acrylate type in drying
Problem Phenomenon
Polybutyl acrylate-type PBAK exhibited low peel strength during drying processing at 80-150°C.
Cause Analysis
Improper crosslinking degree of PBAK caused the problem.
Solution
Improve the drying method.
Key Takeaway
PBAK for coating and adhesive applications requires fine formulation design.