Injection Molding
6 조회수
POE surface orange peel
문제 현상
POE product surface orange-peel-like uneven texture, rough hand feel
원인 분석
Mold temperature too low <30°C, product surface rapidly cools and solidifies, then the interior continues to shrink causing surface unevenness; injection speed too low
해결 방법
1) Raise mold temperature to 40-50°C to delay surface solidification; 2) Appropriately increase injection speed; 3) Increase holding pressure to reduce internal shrinkage
핵심 요약
Orange peel is caused by rapid cooling and solidification; raising mold temperature and holding pressure are key
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다