Material Analysis
11 조회수
High density of PET extruded foamed sheet
문제 현상
PET foamed sheet density higher than target value (e.g., >0.5g/cm³), unsatisfactory weight reduction effect.
원인 분석
Insufficient foaming agent addition or incomplete decomposition, foaming temperature too low with insufficient gas expansion, insufficient melt strength with gas escaping.
해결 방법
Increase foaming agent dosage or switch to high-efficiency foaming agent; increase foaming temperature; use chain extenders to increase melt strength; optimize the die head.
핵심 요약
PET foaming density control requires synergy of melt strength, foaming agent, and process.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!