Extrusion & Post
4 조회수
Poor adhesion of electrostatic spraying on PET products
문제 현상
The adhesion of electrostatically sprayed coating on the surface of PET products is insufficient, and the coating peels off.
원인 분석
Poor PET surface conductivity causes uneven charge accumulation during electrostatic spraying, and coating powder adhesion is poor.
해결 방법
Apply a conductive primer to the product surface; appropriately increase baking temperature to bond the coating with the substrate; preheat the product.
핵심 요약
PET electrostatic spraying requires conductive pretreatment to obtain good results.
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다