Extrusion & Post
8 visualizaciones
Poor adhesion of electrostatic spraying on PET products
Fenómeno del problema
The adhesion of electrostatically sprayed coating on the surface of PET products is insufficient, and the coating peels off.
Análisis de la causa
Poor PET surface conductivity causes uneven charge accumulation during electrostatic spraying, and coating powder adhesion is poor.
Solución
Apply a conductive primer to the product surface; appropriately increase baking temperature to bond the coating with the substrate; preheat the product.
Conclusión clave
PET electrostatic spraying requires conductive pretreatment to obtain good results.
¿Le ha resultado útil?
0 personas encontraron esto útil