Extrusion & Post 7 visualizações

Poor adhesion of electrostatic spraying on PET products

Fenómeno do problema
The adhesion of electrostatically sprayed coating on the surface of PET products is insufficient, and the coating peels off.
Análise das causas
Poor PET surface conductivity causes uneven charge accumulation during electrostatic spraying, and coating powder adhesion is poor.
Solução
Apply a conductive primer to the product surface; appropriately increase baking temperature to bond the coating with the substrate; preheat the product.
Conclusão principal
PET electrostatic spraying requires conductive pretreatment to obtain good results.
PETelectrostatic sprayingadhesionconductive primer