메뉴
재료 기계
인사이트
기사 동영상 문제 및 해결책
About
Chembull 소개 미디어 파트너
문의하기
언어
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어

문제 및 해결책

일반적인 플라스틱 재료 문제에 대한 실질적인 답변

11636 질문
Q
POE extrusion feeding unstable
A
Feeding instability is caused by pellet characteristics; loss-in-weight feeding and anti-bridging are the core
Extrusion & Post POE feedingbridgingloss-in-weight feedergranulationfeeding screw
Q
POE film printing adhesion poor
A
Poor printing adhesion is caused by insufficient surface polarity; corona treatment and special ink are key
Extrusion & Post POE filmprinting adhesioncorona treatmentspecial inksurface tension
Q
POE extrusion film thick edges and thin middle
A
U-shaped thickness is caused by die flow channel and swell difference; coat-hanger die and gap fine adjustment are key
Extrusion & Post POE filmthickness distributioncoat-hanger diegap fine adjustmentedge effect
Q
POE and color masterbatch mixing color uneven
A
Color masterbatch carrier matching and full dispersion are the key to color uniformity
Injection Molding POE coloringcolor masterbatchcarrier compatibilitypigment dispersioncolor streaks
Q
POE extrusion surface rough
A
Surface roughness is caused by low-temperature extrusion and die defects; raising temperature and polishing the die are core countermeasures
Extrusion & Post POE extrusionsurface roughnessdie polishingextrusion temperaturemelt elasticity
Q
POE extruder screw severe wear
A
Screw wear is caused by filler friction and adhesion; wear-resistant screw and temperature control are key
Extrusion & Post POE extrusionscrew wearnitrided screwfiller frictionbimetallic screw
Q
POE injection molded product oil spots
A
Oil spots are caused by external sources of release agent and lubricant; reducing release agent and sealing mold lubrication are key
Injection Molding POE injectionoil spotsmold release agentlubricant exudationmold sealing
Q
POE '2079851475616104452 weld line strength low
Q
POE '2079851475616104452 flow length ratio insufficient
A
Insufficient flow length ratio is caused by high POE viscosity; high temperature, high pressure and large gate are key
Injection Molding POE injectionflow length ratiomelt viscosityinjection temperatureflow aid
Q
POE extrusion pipe inner wall rough
A
Pipe inner wall roughness is caused by mandrel condition and insufficient cooling; polishing mandrel and internal cooling are key
Extrusion & Post POE pipeinner wall roughnessmandrel polishinginternal coolingmelt elasticity