Extrusion & Post
3 views
ASA FDM printing temperature
Problem Phenomenon
[Problem phenomenon] ASA filament printing nozzle clogging, weak interlayer or deformation, temperature parameters confused
Cause Analysis
ASA FDM extrusion temperature 240-270°C (eSUN) or 245-265°C (3DTrcek), bed temperature 90-110°C and enclosed chamber required; temperature too low weak interlayer, too high degradation and strong odor
Solution
Extrusion temperature start optimization from 245-265°C; bed temperature 90-110°C; enclosed chamber reduces warpage; fan 0% or minimal cooling; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Key Takeaway
ASA printing 245-265°C with 90-110°C bed temperature, chamber indispensable; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
Was this helpful?
0 people found this helpful