Blow Molding 2 views

LDPE '2079851475616104457 Temperature

Problem Phenomenon
LDPE '2079851475616104457 parison sagging.
Cause Analysis
High parison temperature gives low melt strength; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; This mechanism has been repeatedly verified by industry literature and should be confirmed first during troubleshooting.
Solution
Take the lower limit of parison temperature; match extrusion speed; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; Change only one variable at a time and record parameter changes to facilitate locating effective measures.
Key Takeaway
Parison sagging is controlled by the temperature lower limit; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; Incorporate this case into the defect archive as a troubleshooting reference for similar future problems.
LDPE'2079851475616104457parisonsagging