Problem Phenomenon
Drying is qualified but occasional haze still occurs in blowing.
Cause Analysis
After drying, preforms are re-moistened by exposure in humid environments; open conveying process.
Solution
①Sealed conveying after drying; ②shorten exposure time; ③hopper heat preservation.
Key Takeaway
Preventing re-moistening = the second half of drying.
PET; drying; re-moistening; sealing; conveying