PET Preform Re-Moistening After Drying
Fenómeno do problema
Drying is qualified but occasional haze still occurs in blowing.
Análise das causas
After drying, preforms are re-moistened by exposure in humid environments; open conveying process.
Solução
①Sealed conveying after drying; ②shorten exposure time; ③hopper heat preservation.
Conclusão principal
Preventing re-moistening = the second half of drying.