Injection Molding 9 views

PMMA Injection Product Weld Line Whitening

Problem Phenomenon
White line at the confluence.
Cause Analysis
Cold flow front + air inclusions.
Solution
①Raise temperature; ②venting; ③overflow well.
Key Takeaway
White line = cold flow front.
PMMA; weld line; whitening; venting