Injection Molding 4 views

POM '2079851475616104452 cycle too long

Problem Phenomenon
Slow cycle.
Cause Analysis
Crystallization is fast but thick-wall cooling still takes time; water line efficiency is low.
Solution
①Optimize water lines; ②reduce material in thick walls; ③balance mold temperature and cycle.
Key Takeaway
Cycle = cooling efficiency.
POM;cycle;cooling;water lines