Injection Molding 4 views

PP Injection Part Gloss Deficiency

Problem Phenomenon
PP parts are overall dull and not bright.
Cause Analysis
Low mold temperature and insufficient holding pressure cause poor surface replication; low mold polish grade; some grades are inherently matte.
Solution
①Raise mold temperature and holding pressure; ②upgrade cavity polishing; ③confirm grade gloss characteristics; ④improve venting.
Key Takeaway
Gloss = replication + mold + grade, three elements.