Molds & Tooling 2 views

TPE Mold Temperature Effect on Surface

Problem Phenomenon
The surface gloss of TPE products is unstable
Cause Analysis
Mold temperature fluctuation affects surface replication; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience; this mechanism has been repeatedly verified by industry information and should be confirmed first during troubleshooting
Solution
Lock the mold temperature; maintain water channels; take the upper limit of mold temperature for surface-demanding parts; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Key Takeaway
Surface gloss relies on mold temperature stability; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
TPE mold temperature gloss stability