Menu
Materiais Máquinas
Perspetivas
Artigos Vídeos Problema e solução
About
Sobre a Chembull Parceiros de média
Contacte-nos
Idioma
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Voltar a Problema e solução
Molds & Tooling 7 visualizações

TPE Mold Temperature Effect on Surface

Fenómeno do problema
The surface gloss of TPE products is unstable
Análise das causas
Mold temperature fluctuation affects surface replication; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience; this mechanism has been repeatedly verified by industry information and should be confirmed first during troubleshooting
Solução
Lock the mold temperature; maintain water channels; take the upper limit of mold temperature for surface-demanding parts; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusão principal
Surface gloss relies on mold temperature stability; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
TPE mold temperature gloss stability

Isto foi útil?

0 pessoas acharam isto útil

ChemAI