Material Analysis 9 views

CPE Thermal Decomposition Above 190C

Problem Phenomenon
Temperature exceeding 190C causes violent decomposition and blackening
Cause Analysis
Chlorine atoms are removed from the main chain, producing HCl
Solution
Strictly control the processing temperature not to exceed 190C
Key Takeaway
Temperature is the red line for CPE processing