Injection Molding 3 views

EEA Surface Orange Peel

Problem Phenomenon
Orange-peel-like uneven texture on the surface of EEA products, rough to the touch
Cause Analysis
Mold temperature low <30°C; after the product surface cools and solidifies rapidly, the interior continues to shrink, causing surface unevenness; injection speed too low
Solution
1) Increase mold temperature to 40-50°C to delay surface solidification; 2) Appropriately increase injection speed; 3) Increase holding pressure to reduce internal shrinkage
Key Takeaway
Orange peel is caused by rapid cooling and solidification; increasing mold temperature and holding pressure are key
EEA orange peel mold temperature holding pressure surface solidification