Extrusion & Post 8 views

Complex cross-section profile dimension control difficult

Problem Phenomenon
Complex cross-section profile dimension control difficult
Cause Analysis
Profile cross-section complex, cooling shrinkage differences in all directions are large Improper sizing sleeve design, dimensional deviation Haul-off speed and extrusion speed not matched, tensile deformation Insufficient cooling and sizing, dimensions change over time Cellulose acetate butyrate shrinkage rate 0.4-0.6% requires precise sizing sleeve design
Solution
Precisely design the sizing sleeve according to the 0.4-0.6% shrinkage rate Optimize cooling to ensure uniformity in all directions Precisely match haul-off and extrusion speeds Fully cool and size to prevent dimensional changes Complex cross-sections require multi-stage sizing
Key Takeaway
Profiles require precise sizing sleeves and sufficient cooling
profilesizing sleeveshrinkage ratecooling