Extrusion & Post
14 visualizaciones
Complex cross-section profile dimension control difficult
Fenómeno del problema
Complex cross-section profile dimension control difficult
Análisis de la causa
Profile cross-section complex, cooling shrinkage differences in all directions are large
Improper sizing sleeve design, dimensional deviation
Haul-off speed and extrusion speed not matched, tensile deformation
Insufficient cooling and sizing, dimensions change over time
Cellulose acetate butyrate shrinkage rate 0.4-0.6% requires precise sizing sleeve design
Solución
Precisely design the sizing sleeve according to the 0.4-0.6% shrinkage rate
Optimize cooling to ensure uniformity in all directions
Precisely match haul-off and extrusion speeds
Fully cool and size to prevent dimensional changes
Complex cross-sections require multi-stage sizing
Conclusión clave
Profiles require precise sizing sleeves and sufficient cooling
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!