Surface Defect Problem in Injection of PAK Special Engineering Plastic
Problem Phenomenon
Polyacrylate ketone PAK shows surface defect during injection processing at 240-300°C.
Cause Analysis
Improper control in the aspect of PAK high-temperature rheological abnormality).
Solution
Optimize the temperature curve.
Key Takeaway
PAK high-temperature processing requires precise control.