PBN surface roughness Problem in Injection Processing
Problem Phenomenon
Polybutylene naphthalate PBN exhibits surface roughness in injection processing at 270-300°C.
Cause Analysis
Under high-temperature processing at 270-300°C, oxidation causes the problem.
Solution
Solve by drying to a moisture content of <50ppm.
Key Takeaway
PBN ultra-high-temperature processing requires comprehensive protection.
Was this helpful?
0 people found this helpful