LCP bonding with metal inserts
Problem Phenomenon
Bonding strength of LCP overmolding metal inserts in '2079851475616104452.
Cause Analysis
Under LCP high mold temperature processing, metal inserts need preheating to avoid debonding from cold-hot shrinkage.
Solution
Preheat inserts to >150°C; groove the surface to increase anchoring.
Key Takeaway
Bonding of LCP with metal requires preheating and surface treatment.