SIS '2079851475616104452 cycle too long affecting efficiency
Problem Phenomenon
2079851475616104452 cycle exceeds the target by more than 20%
Cause Analysis
Cooling time accounts for a large proportion, insufficient plasticization, slow mold opening and closing
Solution
Optimize cooling water channels, increase plasticizing capacity, improve mold opening and closing
Key Takeaway
Cycle optimization is the key to increasing output and reducing cost