Extrusion & Post 2 views

Haul-off speed mismatch of heat-resistant polyethylene extruded products

Problem Phenomenon
The extrudate is uneven in thickness; when the haul-off is too fast the product becomes thinner and narrower, and when the haul-off is too slow the product becomes thicker and wider. Mismatch between haul-off speed and extrusion speed causes product dimensional deviation.
Cause Analysis
(1) Haul-off speed setting does not match extrusion speed (2) Haul-off machine slips, actual haul-off speed unstable (3) Haul-off clamping force insufficient or excessive (4) Extrusion speed fluctuation makes haul-off difficult to synchronize (5) Haul-off control system responds slowly
Solution
(1) Adjust haul-off speed to match extrusion speed, determine synchronous speed by weighing method (2) Check haul-off tracks or rollers to ensure no slipping, replace clamping pads if necessary (3) Adjust haul-off clamping force to ensure uniform clamping without damaging the product (4) Stabilize extrusion speed, reduce fluctuation (5) Upgrade the haul-off control system to improve response speed and accuracy
Key Takeaway
Haul-off speed mismatch needs to be solved by precisely adjusting haul-off parameters and ensuring haul-off stability.
haul-off speedspeed matchinghaul-off slippageclamping forcehaul-off control