Injection Molding 9 views

High temperature resistance requirements of PAR '2079851475616104452 machines and molds

Problem Phenomenon
Conventional '2079851475616104452 machines and molds are difficult to withstand the PAR 280-320°C processing temperature for a long time.
Cause Analysis
The strength of equipment and mold materials decreases at high temperature, and the service life is shortened.
Solution
Use high-temperature-grade '2079851475616104452 machines; select heat-resistant stainless steel for the mold steel.
Key Takeaway
The high-temperature requirements of PAR for equipment must be matched.
PAR'2079851475616104452 machinemold steelhigh temperature