Problem Phenomenon
After adding flame retardants, the melt flowability of PBT decreases and the injection mold filling pressure increases.
Cause Analysis
The filling amount of flame retardants (such as brominated + antimony trioxide) is large (15-25%), increasing the melt viscosity; some flame retardants have poor thermal stability and decompose at high temperature.
Solution
Select high-efficiency flame retardants to reduce the filling amount; appropriately raise the processing temperature; add lubricating dispersants.
Key Takeaway
PBT flame retardancy needs a balance between flame retardancy and processability.