Injection Molding 9 views

Difficulty in Removing Flash from PBT Injection-Molded Products

Problem Phenomenon
The product flash is thin and tough, making manual removal difficult.
Cause Analysis
PBT has good toughness; the flash is not brittle and is not easy to break off; although the flash thickness is thin, its strength is high.
Solution
Reduce flash generation (increase the clamping force and reduce the injection pressure); use automatic deflashing equipment (cryogenic deflashing).
Key Takeaway
PBT flash has good toughness and high removal cost.
PBTflashremovalcryogenic deflashing