Injection Molding 2 views

Excessively fast screw wear of PET '2079851475616104452 machine

Problem Phenomenon
When processing glass fiber containing PET, the screw and barrel of the '2079851475616104452 machine wear severely, and their life is greatly shortened.
Cause Analysis
Glass fiber is extremely abrasive to metal surfaces; the screw and barrel materials are not wear-resistant (not bimetallic treated).
Solution
Use bimetallic screws and barrels (surface hardness above HRC60); reduce glass fiber content; appropriately reduce processing temperature.
Key Takeaway
Reinforced PET processing requires wear-resistant special screws and barrels.
PETglass fiber reinforcementscrew wearbimetallicabrasion