PETG flame retardant formulation poor processability

Problem Phenomenon
After adding flame retardant, the melt flowability decreases significantly, making injection filling difficult.
Cause Analysis
The flame retardant filling amount is large affecting flowability, and the flame retardant has poor compatibility with PETG.
Solution
Select a flame retardant system with little impact on flowability (phosphorus-based); add lubricant; appropriately increase the processing temperature.
Key Takeaway
PETG flame retardant modification needs to balance flame retardancy and processability.