Material Drying 2 views

Bubbles in PLA '2079851475616104452 after moisture absorption

Problem Phenomenon
Bubbles appear on the surface and inside of PLA products.
Cause Analysis
PLA has strong hygroscopicity; when drying is insufficient, the moisture content is high (>500ppm), and water vapor produces bubbles during processing.
Solution
Drying conditions: 60-80°C/4-6h (amorphous grade) or 80-100°C/2-3h (crystalline grade) to moisture <250ppm.
Key Takeaway
The hygroscopicity of PLA is the first obstacle to processing quality.