Extrusion & Post 7 visualizações

LDPE Film Printing Ink Adhesion

Fenómeno do problema
Printing ink adhesion is poor, and color comes off after rubbing.
Análise das causas
Insufficient surface energy or inadequate corona treatment; slip agent migration on the film surface also hinders ink wetting.; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
Solução
①Increase corona treatment intensity; ②Control slip agent dosage; ③Test dyne value before printing; ④Select matching ink.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
Conclusão principal
Printing quality starts with surface energy management; dyne value testing is the basis for release.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; Incorporate this case into the defect archive as a troubleshooting reference for similar future problems.