Extrusion & Post 3 visualizaciones

LDPE Film Printing Ink Adhesion

Fenómeno del problema
Printing ink adhesion is poor, and color comes off after rubbing.
Análisis de la causa
Insufficient surface energy or inadequate corona treatment; slip agent migration on the film surface also hinders ink wetting.; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
Solución
①Increase corona treatment intensity; ②Control slip agent dosage; ③Test dyne value before printing; ④Select matching ink.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
Conclusión clave
Printing quality starts with surface energy management; dyne value testing is the basis for release.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; Incorporate this case into the defect archive as a troubleshooting reference for similar future problems.
LDPE; film; printing; adhesion; surface energy; corona