Processing Machinery 6 visualizações

PA66 product shrinkage rate out of tolerance

Fenómeno do problema
Overall dimensional deviation, poor assembly.
Análise das causas
Shrinkage 1.5%~2.5% value selection improper; holding has great influence; wall thickness differences also cause deviation; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience.
Solução
①Measure actually and repair the mold; ②optimize holding pressure and switchover point, taking into account both feeding and internal stress; ③unify measurement state; ④measure shrinkage by wall thickness and repair the mold with differentiated compensation; ⑤use CAE analysis to assist decision-making when necessary.
Conclusão principal
PA66 dimension='measured correction': shrinkage rate measured by wall thickness, differentiated compensation; unified measurement state is the premise; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
PA66; shrinkage rate; dimension; holding pressure