Production & Quality 5 visualizações

PCABS back pressure adjustment

Fenómeno do problema
PC/ABS back pressure too high, shear heat, reduce in 50psi steps, observe 10+ cycles.
Análise das causas
PC/ABS back pressure too high, shear heat degrades heat-sensitive materials; reduce in 50psi steps; observe 10+ cycles per adjustment; heat silver streak troubleshooting; shear heat management.
Solução
①Reduce back pressure in 50psi steps; ②observe 10+ cycles; ③heat silver streak troubleshooting; ④shear heat management; ⑤melt temperature monitoring.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusão principal
The step adjustment and observation cycles of PCABS back pressure are fine craftsmanship; shear heat management protects the material; monitoring prevents degradation.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence