Material Analysis 14 visualizações

Filling Speed and Shear Darkening of PEEK

Fenómeno do problema
[Problem Phenomenon] PEEK thin-wall parts freeze and short-shot when filling is slow, and the melt shears, darkens, and discolors when filling is fast
Análise das causas
A filling time of 1-3 seconds is the conventional target: too slow and the front freezes into a short shot, too fast and shear heating darkens the melt; products below 150 grams are especially sensitive; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind adjustment based solely on experience
Solução
Adjust the filling time toward the 1-3 second target; for thin-wall short shots, prioritize raising mold temperature and nozzle temperature; for shear darkening, reduce speed and check whether the gate size is too narrow; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusão principal
1-3 second filling is the rhythm benchmark of PEEK — check one end each for short shot and darkening; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
filling time shear darkening short shot thin wall