Molding Process 4 visualizações

PET melt pump pressure stabilization

Fenómeno do problema
Sinusoidal periodic fluctuations appear in sheet thickness, which the automatic thickness measurement system cannot completely eliminate
Análise das causas
Slight fluctuations in melt pump speed appear as sinusoidal thickness bands; wear of the pump drive coupling introduces torsional oscillation; the closed-loop thickness measurement system can track it but cannot remove the upstream disturbance
Solução
① Check the melt pump drive coupling for wear; ② control pump speed fluctuation within 0.5%; ③ independently zone-heat the die bolts to control expansion; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusão principal
The melt pump is the heart of PET sheet thickness stability; upstream fluctuations must be eliminated at the source, and downstream closed-loop is only a remedy; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence