Molds & Tooling 6 visualizações

PSU Wall Thickness Design Constraints

Fenómeno do problema
PSU products designed with too thin wall thickness cause filling difficulty and insufficient strength; mold scrap losses after design changes are large.
Análise das causas
PSU melt has poor flowability; the ratio of melt flow length to wall thickness is only about 80; product wall thickness must not be less than 1.5mm, mostly above 2mm; thin-wall design is inherently infeasible.
Solução
①In the design stage, wall thickness not less than 1.5mm, recommended above 2mm; ②Check the flow length ratio at 80; ③For thin-wall requirements, switch to high-flow grades or materials; ④Material review before mold design.
Conclusão principal
PSU wall thickness constraints are hard boundaries determined by material flowability; the 1.5mm bottom line cannot be broken; advancing design review avoids mold waste.; After confirming effectiveness, solidify the parameters and practices into the work instructions to prevent recurrence
PSU; wall thickness; flow length ratio; 1.5mm; design; flowability