Molding Process 3 visualizações

Coarse internal crystallization of EAA

Fenómeno do problema
The spherulites inside EAA products are coarse >50μm, causing reduced transparency and low impact
Análise das causas
Cooling rate too slow <5°C/min allows spherulites to fully grow; no nucleating agent used to control crystallization
Solução
1) Increase the cooling rate to >20°C/min to refine spherulites; 2) Add 0.2-0.3wt% nucleating agent to control crystallization; 3) Lower the mold temperature to accelerate cooling
Conclusão principal
Coarse crystallization is caused by slow cooling; fast cooling and nucleating agent are the key
EAA coarse crystallization spherulite refinement nucleating agent cooling rate